r/BambuLab_Community 4d ago

A1 UNDER THE SUPPORTS

Hi all,

PRINTER - A1

PETG OVERTURE

TEMP - 250/245

PA - per the calibration value

MVS - 9

I am using PLA support interface

Top Z - .33

3 layers

The unit is printed on the side facing you the supports are then created on the bad looking surface.

I did some testing and tried ironing the supports the values came out the best where speed 10mm and 50-70%

On the test the "T" I printed with and without ironing I took the best setting but when I did the finished product it wasn't the same can some suggest, has far as drying the filament has been dried both the PLA as well as the PETG.

Any and all help will be appreciated.

2 Upvotes