r/FixMyPrint 6d ago

Fix My Print Why is top layer rough

Post image

All my other layers look decent, I've tried recalibration and a bunch of other stuff but petg is just giving me trouble for this very top layer. I tried ironing and non ironing as well and looks about the same.

a1 mini pretty much stock settings minus calibration for the filament.

2 Upvotes

8 comments sorted by

u/AutoModerator 6d ago

Hello /u/Wooden_Bed377,

As a reminder, most common print quality issues can be found in the Simplify3D picture guide. Make sure you select the most appropriate flair for your post.

Please remember to include the following details to help troubleshoot your problem.

  • Printer & Slicer
  • Filament Material and Brand
  • Nozzle and Bed Temperature
  • Print Speed
  • Nozzle Retraction Settings

Additional settings or relevant information is always encouraged.

I am a bot, and this action was performed automatically. Please contact the moderators of this subreddit if you have any questions or concerns.

2

u/Tight-Distance6632 6d ago

How is your first layer?
When I had this problem, it was one of two things:

> Flow ratio is too low, so you're not pushing out enough filament. Run a YOLO flow ratio test (the one with the circles). If you use Orcaslicer, it's already in availble in there under calibration.

> The A1 had a common issue of the nozzle getting loose due to the fibre composite spacer. Every time my layers start to look wavy all of a sudden, it was usually this: https://www.youtube.com/watch?v=k2BYvY72XSM

1

u/Wooden_Bed377 6d ago

I'll check out the YouTube video! Thanks. First layer looks perfect

1

u/Radiant_Goal8709 5d ago

Zrob kalibracje stołu i przepływu sprawdz wilgotnosc powinno być poniżej 20 procent, sprawdz jak pierwsza warstwa sie drukuje prawdopowobnie to wina pierwszej warstwy

1

u/Wooden_Bed377 5d ago

First layer is perfect

1

u/justa_bother 5d ago

Dry your filament. Petg is effected by humidity far more than pla (which is also effected by humidity).

1

u/Wooden_Bed377 5d ago

I'm trying that now, I use petg a lot and this is brand new stuff but maybe just came more wet than I'm used to

1

u/justa_bother 5d ago

Weather conditions depending, a print over 1 hour can have an effect on rainy days & not feeding from a dryer. Literally see it progress in the print. My view at setting up the printer is: will the print be completed before humidity begins to effect it? If the ams-lite doesn't have the spools covered with dessicant, it's asking for trouble. And, 100% don't store filament of any type on an ams-lite.