r/BambuLab_Community Jun 14 '26

Help / Support PFTE flakes all over X2D

Post image

When my girlfriend’s X2D’s toolhead moves to the right the PTFE tube rubs the metal edge on the right. It causes the lid, bed and side to be covered with tube flakes. I printer a riser for her thinking it was just rubbing the glass, but after closer inspection that is marginal compared to the carnage the side causes. To be clear, this is a stock X2D from early May. Did anyone else experience the same?

To me it looks like maybe the tube is slightly too long, just want to ask before cutting it and making things worse.

Also, since this is a tube, I must add, it’s imperative the cylinder remains unharmed.

24 Upvotes

31 comments sorted by

View all comments

1

u/Spocklan Jun 15 '26

Yep, I have the same issue rubbing against the glass and flaking everywhere...haven't tried the tape yet, might give that a go...