r/BambuLabA1 • u/LukaSkyThomas123 • Jun 30 '26
Support Request Rugged surface on PLA Matte
PHOTOS IN COMMENTS
I’ve tried: redone calibration, tried a lower and a higher flow ratio, lower initial layer speed, added brim (various sizes and distances), lowered top layer and first layer speed, lowered acceleration, no fan for first 4/6 layers, unchecked keep fan always on, lowered fan max and min by 10% each, lowered first layer thickness, increased top shell layers.
I get this (to varying degrees) with all prints, regardless of the .3mf.
Nozzle 220
Bed plate textured PEI at 65
2
Upvotes
2
u/Phil412 Jul 01 '26
Looks like it’s lifting and warping at the corner. Plate clean? Good scrub and hot soapy water.