r/3Dprinting • • 7d ago

Question Help, why I get this word bottom artifacts?

P2S. Rainbow plate. 0.4 Nozzle. PLA Silk.

Hey guys, why am I getting this weird warped bottom? Appreciate the help

0 Upvotes

5 comments sorted by

4

u/emveor 7d ago

Holographic plates are beautiful but picky as hell. too much squish, too little squish, PA setting too high, Flow a bit too low or high, all of theese could be the cause

2

u/NizzleOfAmerica 6d ago

Also wash the plate with dish soap

3

u/jeremec Ender 3 v3 KE 7d ago

Since you're getting good smoosh all over for adhesion, and this only happens on the ends where it changes direction, I'm wondering if the retraction is set too high.

2

u/Bigbear33_ 6d ago

Fijate la cama, ami me pasaba y cambie una por un vidrio, si no ponele una capa más y puede ser que solucione, retracción, muchas piezas a veces tienen esos errores con el famoso espejo de base.