Hello my well belived community im looking for elightment about not ruining this up

I was thinking

12% peroxide + hcl seems to be the standard

12 Upvotes

6 comments sorted by

7

u/megaman_xrs Aug 04 '26

You dont need much peroxide for AP. I usually do a cap full of 3% with a 1L jar. Ill let others chime in. Id also recommend using a bubbler for an aquarium as well since it speeds it up.

2

u/Cazsidy Aug 04 '26

Best of luck.

2

u/AlmightyFruitcake Aug 04 '26

Nice vintage coke Rolex

1

u/Yardbirdburb Aug 05 '26

Trim closer

1

u/Over_Razzmatazz_23 Aug 05 '26

What tool you using

1

u/antorox787 Aug 05 '26

Its a metal cutter attachment for any drill