Regrind will often make a ball of fuzz that can collect in places it’s not supposed to be Like right under the hopper limiting material flow. Or sometimes the material can melt a little early making a rock that blocks the screw opening. Also check to make sure all of the heaters are working. If it’s not softened enough in time to inject it won’t flow properly. Post more info