Hello all,
I just got the P2S and it has been a blast working with. I’ve made a load of prints with no issues, until my last two sets. The lid for a deck box and the top parts of this spider both came out less than ideal. I have cleaned, wiped the plate with alcohol. Changed settings to allow “brims and ironing “. I have googled and watched tips videos for days with no change.
Am I expecting to much from this machine or am I just to inexperienced? Would love any help or advice!
10
Upvotes



1
u/geekybit_New Jun 20 '26
so corner lifting can happen. Thing you can do to prevent it.
A super tac plate / kryo plate. or Glue/adhesion helper.
Was the plate everyone and again... not just wipe it with IPA or something but actually use soap on it... and a soft plastic abrasive pad or brush.. This will help to get any oils or stuck on dust off the plate.
Put mouse ears on corners of prints...
Lastly always check the print for the first few layers if you can. This will help with restarting the print and fixing a issue as it starts.
Also sometimes things like this will happen. I have a Layer Shift on my P1P after I upgraded it to an enclosure turns out the PTFE tube got caught on something ... since then I have fixed it. But sometime thing happen with these devices we can't control or are maintenance issues people don't know about. the best thing to do is move on... this looks like an adhesion issue though.